TABLE 1 Plate Materials
CM-65 carbon-molybdenum steel A204/A204M A 201
CM-70 carbon-molybdenum steel A204/A204M B 201
CM-75 carbon-molybdenum steel A204/A204M C 201
CMSH-70 carbon-manganese-silicon steel, normalized A537/A537M 1  
CMS-75 carbon-manganese-silicon steel A299/A299M . . . . . .
CMSH-80 carbon-manganese-silicon steel, quenched and tempered A537/A537M 2  
1 ⁄ 2 CR 1 ⁄ 2 % chromium, 1 ⁄ 2 % molybdenum steel A387/A387M 2 201
1CR 1 % chromium,1 ⁄ 2 % molybdenum steel A387/A387M 12 201
1 1 ⁄ 4 CR 1 1 ⁄ 4 % chromium,1 ⁄ 2 % molybdenum steel A387/A387M 11 201
2 1 ⁄ 4 CR 2 1 ⁄ 4 % chromium, 1 % molybdenum steel A387/A387M 22 201
3CR 3 % chromium, 1 % molybdenum steel A387/A387M 21 201
5CR 5 % chromium,1 ⁄ 2 % molybdenum steel A387/A387M 5 225
9CR 9 % chromium, 1 % molybdenum steel A387/A387M 9 241
91 9 % chromium, 1 % molybdenum, vanadium, niobium C A387/A387M 91 B 241

 

TABLE 2 Heat Treatment Parameters A

Post-Weld Heat-Treat









CM-65 A204/A204M 1100 to 1200 [590 to 650] 1700 [925] . . . . . .
CM-70 A204/A204M 1100 to 1200 [590 to 650] 1700 [925] . . . . . .
CM-75 A204/A204M 1100 to 1200 [590 to 650] 1700 [925] . . . . . .
CMSH-70 A537/A537M 1100 to 1200 [590 to 650] 1700 [925] . . . . . .
CMS-75 A299/A299M 1100 to 1200 [590 to 650] 1700 [925] . . . . . .
CMSH-80 A537/A537M 1100 to 1200 [590 to 650] B 1700 [925] 1100 to 1250 [590 to 675]
1 ⁄ 2 CR A387/A387M 1100 to 1300 [590 to 705] 1850 [1010] 1700 [925] 1150 to 1375 [620 to 745]
1CR A387/A387M 1100 to 1350 [590 to 730] 1850 [1010] 1700 [925] 1150 to 1375 [620 to 745]
11 ⁄ 4 CR A387/A387M 1100 to 1375 [590 to 745] 1850 [1010] 1700 [925] 1150 to 1375 [620 to 745]
21 ⁄ 4 CR A387/A387M 1200 to 1400 [650 to 760] 1850 [1010] 1700 [925] 1250 to 1400 [675 to 760]
3CR A387/A387M 1200 to 1400 [650 to 760] 1850 [1010] 1700 [925] 1250 to 1400 [675 to 760]
5CR A387/A387M 1200 to 1400 [650 to 760] 1850 [1010] 1650 [900] 1300 to 1400 [705 to 760]
9CR A387/A387M 1325 to 1375 [715 to 745] C . . . 1325 to 1375 [715 to 745]
91 A387/A387M 1350 to 1420 [730 to 770] 1900 to 2000[1040 to 1095] 1900 min[1040 min] 1350 to 1440 [730 to 780]

 



10
11 9
12 9 8.3
13 8.3
20 stress relieved, see 5.3.1
21 stress relieved, see 5.3.1 9
22 stress relieved, see 5.3.1 9 8.3
23 stress relieved, see 5.3.1 8.3
30 normalized, see 5.3.2
31 normalized, see 5.3.2 9
32 normalized, see 5.3.2 9 8.3
33 normalized, see 5.3.2 8.3
40 normalized and tempered, see 5.3.3
41 normalized and tempered, see 5.3.3 9
42 normalized and tempered, see 5.3.3 9 8.3
43 normalized and tempered, see 5.3.3 8.3
50 quenched and tempered, see 5.3.4
51 quenched and tempered, see 5.3.4 9
52 quenched and tempered, see 5.3.4 9 8.3
53 quenched and tempered, see 5.3.4 8.3